about-us(1)

Products

Low price for Tensile Fixture - Slow strain rate stress corrosion tester – Enpuda


Product Detail

Product Tags

Related Video

Feedback (2)

We're going to commit ourselves to giving our esteemed buyers using the most enthusiastically considerate solutions for Servo Structure Fatigue Testing Machine , Rubber Fatigue Life Measurement , Tensile Testing Machine For Engineering Materials , If you are fascinated in any of our products, you should come to feel no cost to call us for more aspects. We hope to cooperate with a lot more close friends from all over the world.
Low price for Tensile Fixture - Slow strain rate stress corrosion tester – Enpuda Detail:


Slow strain rate stress corrosion tester

APPLICATION AREA


wusf (1)


wusf (2)


wusf (3)


wusf (4)

Slow strain rate (SSRT) stress corrosion (SCC) testing machine is mainly used to simulate the tensile, compression, bending, creep of metal, non-metal, composite materials and their products under different environmental media conditions. Variation test to determine stress corrosion properties of materials under slow rate conditions.

The Panasonic full digital AC servo controller is used to control the Panasonic AC servo motor with high precision and high response frequency to realize the two-stage deceleration of the arc toothed synchronous belt deceleration system and the deceleration system of the reducer, so as to ensure that the stretching speed of the slow strain rate test can be Stepless adjustment between 1×10-1~1×10-6mm/S.

Customized service / Test standard

We not only provide standardized machines, but also customize machines and LOGO according to customer requirements. Please tell us your requirements and we will try our best to meet your needs.

Please provide the test standard you need to our company, our company will help you customize the test machine that meets the test standard you need

Testing machine standard

1. It is manufactured according to GB / t2611-2007 general technical conditions for testing machines and GB / T 16491-2008 electronic universal testing machines;

2. Verification and acceptance shall be carried out according to GB / t12160-2002 “provisions for extensometers for uniaxial test” and GB / t16825-2008 “inspection of tensile testing machines”;

3. It is applicable to GB, JIS, ASTM, DIN and other standards.

Testing standard

Slow Strain Rate Stress Corrosion Tester

Performance features / advantages


Slow strain rate stress corrosion tester (2)

1. Exquisite and elegant design: our company has always attached great importance to the appearance of products and developed many products comparable to foreign models. Some of the testing machines have been protected by national appearance patents;
2. Arc tooth synchronous belt deceleration system: it has the advantages of high efficiency, long life, low noise and maintenance free;
3. High precision ball screw loading: stable loading, long service life, good long-term stability and energy saving;
4. A variety of protection measures: such as electronic limit protection, overcurrent, overvoltage and other electrical protections in power links;
5. Measurement and control system: adopt pure digital phase-locked loop pulse control mode, without falling and misalignment;
6. Simple, reliable and powerful user interface.
7. The open data structure allows users to randomly call both the result parameters and the process data, which is very convenient for scientific research and teaching.
8. User self-editing report function. Data can be easily imported into EXCEL form, which is convenient for users to process later.

Key Parts


SSRT Stamping System

1. SSRT Stamping System

2. High-precision ball screw, high precision, stable operation and long service life


High-precision ball screw, high precision, stable operation and long service life


SSRT high temperature fixture(Design according to the actual needs of users)

3. SSRT high temperature fixture(Design according to the actual needs of users)

4. High-precision load sensor, American Transcell brand


High-precision load sensor, American Transcell brand


Using Japanese Panasonic servo motor, stable and durable performance, high precision

5. Using Japanese Panasonic servo motor, stable and durable performance, high precision


Product detail pictures:

Low price for Tensile Fixture - Slow strain rate stress corrosion tester – Enpuda detail pictures


Related Product Guide:

Each individual member from our large performance revenue crew values customers' needs and company communication for Low price for Tensile Fixture - Slow strain rate stress corrosion tester – Enpuda , The product will supply to all over the world, such as: Cyprus, Honduras, Portland, With excellent solutions, high quality service and sincere attitude of service, we ensure customer satisfaction and help customers create value for mutual benefit and create a win-win situation. Welcome customers all over the world to contact us or visit our company. We'll satisfy you with our qualified service!
  • This is a very professional and honest Chinese supplier, from now on we fell in love with the Chinese manufacturing.
    5 Stars By Matthew Tobias from Slovenia - 2018.07.26 16:51
    This is the first business after our company establish, products and services are very satisfying, we have a good start, we hope to cooperate continuous in the future!
    5 Stars By June from Angola - 2018.06.30 17:29
    Write your message here and send it to us