about-us(1)

Products

China Supplier Astm Tensile Test - Slow strain rate stress corrosion tester – Enpuda


Product Detail

Product Tags

Related Video

Feedback (2)

We emphasize advancement and introduce new products into the market each year for Torque Fatigue Testing Machine , Automobile Suspension System Fatigue Testing Machine , Rebar Tensile Strength Test , At our firm with good quality initially as our motto, we manufacture merchandise that are entirely made in Japan, from materials procurement to processing. This enables them for being used with confident peace of mind.
China Supplier Astm Tensile Test - Slow strain rate stress corrosion tester – Enpuda Detail:


Slow strain rate stress corrosion tester

APPLICATION AREA


wusf (1)


wusf (2)


wusf (3)


wusf (4)

Slow strain rate (SSRT) stress corrosion (SCC) testing machine is mainly used to simulate the tensile, compression, bending, creep of metal, non-metal, composite materials and their products under different environmental media conditions. Variation test to determine stress corrosion properties of materials under slow rate conditions.

The Panasonic full digital AC servo controller is used to control the Panasonic AC servo motor with high precision and high response frequency to realize the two-stage deceleration of the arc toothed synchronous belt deceleration system and the deceleration system of the reducer, so as to ensure that the stretching speed of the slow strain rate test can be Stepless adjustment between 1×10-1~1×10-6mm/S.

Customized service / Test standard

We not only provide standardized machines, but also customize machines and LOGO according to customer requirements. Please tell us your requirements and we will try our best to meet your needs.

Please provide the test standard you need to our company, our company will help you customize the test machine that meets the test standard you need

Testing machine standard

1. It is manufactured according to GB / t2611-2007 general technical conditions for testing machines and GB / T 16491-2008 electronic universal testing machines;

2. Verification and acceptance shall be carried out according to GB / t12160-2002 “provisions for extensometers for uniaxial test” and GB / t16825-2008 “inspection of tensile testing machines”;

3. It is applicable to GB, JIS, ASTM, DIN and other standards.

Testing standard

Slow Strain Rate Stress Corrosion Tester

Performance features / advantages


Slow strain rate stress corrosion tester (2)

1. Exquisite and elegant design: our company has always attached great importance to the appearance of products and developed many products comparable to foreign models. Some of the testing machines have been protected by national appearance patents;
2. Arc tooth synchronous belt deceleration system: it has the advantages of high efficiency, long life, low noise and maintenance free;
3. High precision ball screw loading: stable loading, long service life, good long-term stability and energy saving;
4. A variety of protection measures: such as electronic limit protection, overcurrent, overvoltage and other electrical protections in power links;
5. Measurement and control system: adopt pure digital phase-locked loop pulse control mode, without falling and misalignment;
6. Simple, reliable and powerful user interface.
7. The open data structure allows users to randomly call both the result parameters and the process data, which is very convenient for scientific research and teaching.
8. User self-editing report function. Data can be easily imported into EXCEL form, which is convenient for users to process later.

Key Parts


SSRT Stamping System

1. SSRT Stamping System

2. High-precision ball screw, high precision, stable operation and long service life


High-precision ball screw, high precision, stable operation and long service life


SSRT high temperature fixture(Design according to the actual needs of users)

3. SSRT high temperature fixture(Design according to the actual needs of users)

4. High-precision load sensor, American Transcell brand


High-precision load sensor, American Transcell brand


Using Japanese Panasonic servo motor, stable and durable performance, high precision

5. Using Japanese Panasonic servo motor, stable and durable performance, high precision


Product detail pictures:

China Supplier Astm Tensile Test - Slow strain rate stress corrosion tester – Enpuda detail pictures


Related Product Guide:

We'll make every effort and hard work being outstanding and excellent, and speed up our techniques for standing during the rank of global top-grade and high-tech enterprises for China Supplier Astm Tensile Test - Slow strain rate stress corrosion tester – Enpuda , The product will supply to all over the world, such as: Croatia, Frankfurt, Slovenia, Our market share of our products has greatly increased yearly. If you are interested in any of our products or would like to discuss a custom order, please feel free to contact us. We are looking forward to forming successful business relationships with new clients around the world in the near future. We are looking forward to your inquiry and order.
  • The factory has advanced equipment, experienced staffs and good management level, so product quality had assurance, this cooperation is very relaxed and happy!
    5 Stars By Lydia from India - 2018.12.22 12:52
    It's really lucky to find such a professional and responsible manufacturer, the product quality is good and delivery is timely, very nice.
    5 Stars By Grace from Cyprus - 2017.08.15 12:36
    Write your message here and send it to us